Brand Name : BonTek
Model Number : Lithium Tantalate (LiTaO3)
Certification : ISO:9001, ISO:14001
Place of Origin : China
MOQ : 5 pcs
Price : Negotiable
Payment Terms : T/T
Supply Ability : 10000 pcs/Month
Delivery Time : 1-4 weeks
Packaging Details : Cassette/ Jar package, vaccum sealed
Product : LiTaO3 Wafer
Grade : SAW Grade, Optical Grade
Orientation : Y-cut, 36Y-cut, 42Y-cut
Surface Finish : Double / Single side polish
Dia. : 3inch, 4inch, 6inch
Thickness : 0.35mm, 0.5mm
Primary Flat : 22mm, 32mm, 47.5mm, 57.5mm
Application : High Frequency Broadband Filter and Piezoelectric Transducer
Precision Pyroelectricity: LiTaO3's Impact in Motion Sensors
Witness the impact of LiTaO3's pyroelectric effect in the realm of motion sensors, where precision matters most. Our ultra-thin LiTaO3 wafers, at a wafer-level thickness of 20um and diameters reaching 4 inches, play a transformative role in enhancing the accuracy of motion-sensing applications. The inherent pyroelectric effect responds dynamically to temperature changes, allowing for meticulous detection in security systems and automation technologies. LiTaO3's thinness is not just a feature; it's the key to unlocking unparalleled precision in motion sensor applications.



| Material | Ltihium Tantalate (LT) Wafer | ||
| Diameter | 3inch | 4inch | 6inch |
| 76.2mm | 100mm | 150mm | |
| S/D | 20/10 | 20/10 | 20/10 |
| TTV | <3um | <3um | <5um |
| PLTV | >95% | >95% | >95% |
| Warp | <20um | <40um | <50um |
| BOW | <20um | <30um | <30um |
| Roughness | Ra<0.5nm | Ra<0.5nm | Ra<0.5nm |
| Reduction | Standard White | Standard White | Standard White |
| Doping | Fe doped | Fe doped | Fe doped |
| Properties | LiTaO3 (LT) |
| Crystal Structure | Trigonal,a = 5.154, c = 13.784Å |
| Melting Point | 1650℃ |
| Curie Temperature | 607℃ |
| Transmission Range | 400 – 5000 nm |
| Absorption edge | 270nm |
| Absorption loss | < 0.15 %/cm @ 1064 nm |
| Refractive Index | no=2.176,ne=2.180(at 0.633 µm) |
| no=2.131,ne=2.134(at 1.2 µm) | |
| Density | 7.45g/cm3 |
| Thermal Conductivity | 8.78x 10-7 m2/sec |
| Optical homogeneity | ~10-5 |
| Hardness (Mohs) | 5 |
| Elastic Coefficient | CE11 2.33(X 1011 N/m2) |
| CE33 2.77(X 1011 N/m2) | |
| Dielectric Constant | ε11/ε0 52.7 |
| ε33/ε0 44.5 | |
| Solubility in Water | insoluble in water |
| NLO Coefficients | d33 = 13.8 pm/V |
| d22= 2.4 pm/V | |
| d11= 0.85 pm/V | |
| Electro-Optic Coefficients | r31 =8.4 pm/V, @633nm |
| r22 =20 pm/V, @633nm | |
| r33 =30.5 pm/V, @633nm | |
| Damage Threshold | 2 MW/cm2@532nm |